Incoloy 926 Characteristic:
Incoloy 926 Chemical composition:
Alloy | % | Ni | Cr | Fe | C | Mn | Si | Cu | Mo | N | Ti | P | S |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
926 | Min. | 24 | 19 | Balance | 0.5 | 6.0 | 0.15 | 0.6 | |||||
Max. | 26 | 21 | 0.02 | 2 | 0.5 | 1.5 | 7.0 | 0.25 | 1.2 | 0.03 | 0.01 |
Incoloy 926 Physical properties:
Density | 8.1 g/cm3 |
Melting point | 1320-1390 ℃ |
Incoloy 926 Alloy Minimum Mechanical properties in the room temperature:
Alloy state | Tensile strength Rm N/mm2 | Yield strength RP0.2N/mm2 | Elongation A5 % |
926 | 650 | 295 | 35 |
Incoloy 926 Characteristic:
Incoloy 926 Chemical composition:
Alloy | % | Ni | Cr | Fe | C | Mn | Si | Cu | Mo | N | Ti | P | S |
---|---|---|---|---|---|---|---|---|---|---|---|---|---|
926 | Min. | 24 | 19 | Balance | 0.5 | 6.0 | 0.15 | 0.6 | |||||
Max. | 26 | 21 | 0.02 | 2 | 0.5 | 1.5 | 7.0 | 0.25 | 1.2 | 0.03 | 0.01 |
Incoloy 926 Physical properties:
Density | 8.1 g/cm3 |
Melting point | 1320-1390 ℃ |
Incoloy 926 Alloy Minimum Mechanical properties in the room temperature:
Alloy state | Tensile strength Rm N/mm2 | Yield strength RP0.2N/mm2 | Elongation A5 % |
926 | 650 | 295 | 35 |